Skip to content

ADORPALL N2

Package á 25 g

Metallkeramik-Legierung auf Palladiumbasis,

Due to the current commodity price development, all palladium alloys are published on a daily price basis for the time being. Prices are updated every morning at 10 am.

64,90  excl. VAT

Description

GebrAnw Dentalgrundlegierung Adorpall N2_PCG15M_24.01.2024

Type: Metal-ceramic alloy on the palladium basis, type 4 (extra hard)
acc. DIN EN ISO 22674
Colour: white

 

Applicable scope: Inlays, Onlays
Crowns
Small bridges
Middle-sized bridges
Large-span bridges
Milling, cone and attachment works
Modeling casting

 

Composition: Au 15,40
(mass fraction in %) Pd 52,00
Ag 20,00
In   6,00
Ga   1,00
Ru   0,20
Sn  5,40

 

Technical specifications: Density in g/cm³ 12,0
Vickers hardness HV 5/30 (s)270 (n)270 (a-n)280
Yield strength Rp0,2 in MPa (s)540 (n)540 (a-n)610
Elongation at break in % (s)6 (n)6 (a-n)4
Elastic modulus in GPa 110
Average linear CTE 25 – 500 °C in 10-6 K-1 14,2
Average linear CTE 25 – 600 °C in 10-6 K-1 14,5
Melting interval in °C 1150 – 1270

 

Processing: Preheating temp. of the casting moulds in °C 900
Casting temperature in °C 1420
Crucibles Ceramic
Curing 550°C/15min

 

Suitable solders: Joints before ceramic firing AL 1060 W
Joints after ceramic firing AL 750

 

1) Brief description:

s – self-curing, n – after ceramic firing, a-s – curing from s condition
a-n – curing from n condition

2) All information about cured condition is given according to the alloy:

– Oxide firing 10min/ 960°C + 4x4min/ 960°C for yellow conventional bonding alloys
– Oxide firing 10min/ 980°C + 4x4min/ 980°C for white conventional bonding alloys
– Oxide firing 10min/ 800°C + 4x4min/ 800°C for LFC-systems
Corresponding data are true under these conditions only.

3) The ceramic firing should be carried out according to the manufacturer's instructions.